Figure 78
Fig. 78: 2-D diffraction image of iron foil a few microns thick in aluminium oxide (the pressure medium and thermal insulator) at 45 GPa and 2100 K obtained in 10 minutes using a focused beam of 8 by 15 microns (fwhm).
Fig. 78: 2-D diffraction image of iron foil a few microns thick in aluminium oxide (the pressure medium and thermal insulator) at 45 GPa and 2100 K obtained in 10 minutes using a focused beam of 8 by 15 microns (fwhm).