Fig. 47: Temperature variation of the (3/2, 1/2, 15/4) superlattice reflection of NaV2O5 measured by synchrotron X-ray diffraction. The inset shows the log-log plot of the reduced intensity vs. the reduced temperature t = (TSP T) / TSP .